yer im thinking bit of aluminium mesh and isopon 38, rust treated with hammerties Kurust Gel, left to simmer for 2 hours, then primed with Davids zinc 182 before and after filler, with primer filler over top to glaze with top coat of paint, rubed down gently to remove imperfections in the texture with fine wetn dry, and buffed with a cutting compound, served with a sprinkle of chives and a honey dressing.
only kidding,

im gona cut the rust, package it up and send it back to the Russians, and get some proper fresh metal in!! last time it will mess with me!!!
:smt067
Chris